Today, Boyee Nano mill is grinding lithium iron phosphate. The original material had a particle size of D(90)=10.9μm, and only after 3 hours of grinding, it was reduced to D(90)=0.2μm (200nm).welcome friends with grinding needs to come and test at Boyee.